Ceramitalc No. 1

Description: 325 mesh talc

Oxide Analysis Formula Tolerance
CaO 6.94% 0.15
MgO 29.00% 0.85
Na2O 0.18% -
Al2O3 0.28% -
SiO2 56.80% 1.12
Fe2O3 0.20% -
MnO 0.13% -
LOI 6.46%n/a
Oxide Weight 110.53
Formula Weight 118.16

Notes

No longer available.

Was for use in all ceramic applications where a fine-ground talc will develop higher fired strength than coarser grades. Used as an auxiliary flux in electrical porcelain, hotel china and sanitaryware bodies to lower manufacturing temperatures without narrowing the firing range. In semivitreous dinnerware, it decreases the moisture expansion and increases the thermal expansin, contributing to improved resistnace to crazing in glazes dinnerware.

Related Information

Links

Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Materials Ceramitalc
Hazards Talc Hazards Overview
Talc is invaluable in the ceramics industry, it is used as a glaze and body ingredient and as a parting a release agent in various processes. Is it safe?

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy