1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Zirconium Spinel

Alternate Names: Synthetic zirconium silicate, zinc aluminate spinel

Description: Synthetic zinc–alumina–zirconia–silica opacifier

Formula: ZnO·Al₂O₃·ZrO₂·SiO₂

Oxide Analysis Formula Tolerance
ZnO 22.20% 1.00
ZrO2 33.60% 1.00
Al2O3 27.82% 1.00
SiO2 16.39% 1.00
Oxide Weight 366.70
Formula Weight 366.70

Notes

Zirconium spinel is an older commercial name for a synthetic ceramic material containing zinc, alumina, zirconia and silica, used as a glaze opacifier and color stabilizer. The EPA recognizes the name under “Spinels, aluminum zinc zirconium.”

This zirconium silicate variation had colour-stabilizing abilities (likely with certain colors that benefitted from the presense of zinc, e.g. iron chrome browns). It was often combined with other zirconium opacifiers.

Related Information

Links

Typecodes Opacifier
Opacifiers are powders that turn transparent glazes opaque by various chemical and physical mechanisms (and combinations of mechanisms).
Materials Zircon
Zircon (zirconium silicate) is a hard, dense, refractory ceramic material used to opacify pottery glazes and in refractory products such as kiln washes, crucibl

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy