Silica Sand

Alternate Names: quartz sand

Oxide Analysis Formula Tolerance
SiO2 100.00% 1.00
Oxide Weight 60.10
Formula Weight 60.10

Notes

Often used in clay bodies instead of grog or to augment grog. However, the particle shape should be taken into account. Silica sand particles can be rounded or angular, the latter being more suited to clay bodies. However, the very high thermal expansion of the quartz particles should not be ignored. During temperature changes (like cooling in the kiln), quartz grains act independently in the surrounding brittle matrix, imposing their size changes and weakening the fired item or contributing to dunting.

Silica sand is often used to reduce body firing shrinkage and fired warpage. But it is often better to reduce the flux sourcing material in the body (usually feldspar) instead.

Many grades of natural silica sand have round particles, making them excellent as a lubricant on kiln shelves to enable ware to move while shrinking and prevent it from sticking. Silica sand is also used as a source of SiO2 in the glass industry.

Many sizes and particle shapes of silica sand are available. Colors can range from white to brownish, the latter containing iron. Small amounts of iron or contaminating products can darken the sand considerably. Many industrial silica sands are not suitable for ceramics because of the level of impurity particles they contain.

Fused silica or fused quartz is not the same as silica sand. Silica sand particles are crystalline. Fused silica sand is made by melting quartz and cooling it rapidly, the particles are a glass instead of a crystal.

Related Information


This picture has its own page with more detail, click here to see it.

Examples of some different silica sands

Links

Materials #1 Q-Rok
Materials Grog
Materials Mullite
A highly refractory low-expansion alumino-silicate crystal formed naturally only rarely but produced industrially and within fired kaolin bodies.
Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.
Glossary Dunting
Dunting generally refers to firing cracks that occur in ceramic ware as it is cooled in the kiln. The reason is generally uneven cross section or too rapid cooling.
Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy