Learn how to add a recipe, title it, add lines and change them, set lines to added status, deal with unrecognized materials, enter notes and pictures and print a mix ticket
You can also watch this at Screencast-o-matic.com
Start with an empty account at Insight-live.com.
Click the Add button in the recipe manager.
Click the blue Edit button in the recipe panel and name the glaze Cone 04 Glossy Blue and save it.
Add a recipe line: Gerstley Borate, 50. Click Done Editing.
Click show chemistry. Click the Gerstley Borate and compare the materials chemistry with the calculation chemistry in the recipe.
Click Edit again and add 3 more lines: EPK 30, Silica 20, Cobalt 1.
Click Done Editing and not the red footnote warning that a material was not recognized.
It is the cobalt.
Search cobalt in the materials manager to find the proper name.
Edit the recipe and fix the cobalt and check the chemistry.
Edit again and click the Show More Options link. Set the cobalt to phantom status (not participant in the chemistry) and click the Added checkbox.
Click the Notes edit button and enter a note and close and save that panel.
Note where to upload a picture.
Print a mix ticket for 1500 grams without showing the chemistry.
| Glossary |
Digitalfire Insight-Live
A cloud-hosted ceramics-targeted LIMS (lab info management system). It does glaze chemistry and physical testing the “Digitalfire way”. For technicians, educators, potters and hobbyists. |
| Glossary |
Glaze Recipes
Stop! Think! Do not get addicted to the trafficking in online glaze recipes. Learn to make your own or adjust/adapt/fix what you find online. |
| Media |
How to Paste a Recipe Into Insight-live
If your recipe is on the clipboard, this shows you how to import it into Insight-live and make adjustments after. |
| Articles |
Can We Help You Fix a Specific Problem?
There are lots of resources here to help yourself, but if necessary I can help you individually. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk