Al2O3 | B2O3 | BaO | C | CaO | CO2 | CoO | Cr2O3 | Cu2O | CuO | Fe2O3 | FeO | H2O | K2O | Li2O | LOI | MgO | MnO | MnO2 | Na2O | NiO | O | Organics | P2O5 | PbO | SiO2 | SnO2 | SO3 | SO4 | SrO | TiO2 | V2O5 | ZnO | ZrO | ZrO2

Ag2O | AlF3 | As2O3 | As4O6 | Au2O3 | BaF2 | BeO | Bi2O3 | CaF2 | CdO | CeO2 | Cl | CO | CrO3 | Cs2O | CuCO3 | Dy2O3 | Er2O3 | Eu2O3 | F | Fr2O | Free SiO2 | Ga2O3 | GdO3 | GeO2 | HfO2 | HgO | Ho2O3 | In2O3 | IrO2 | KF | KNaO | La2O3 | Lu2O3 | Mn2O3 | MoO3 | N2O5 | NaF | Nb2O5 | Nd2O3 | Ni2O3 | OsO2 | Pa2O5 | PbF2 | PdO | PmO3 | PO4 | Pr2O3 | PrO2 | PtO2 | RaO | Rb2O | Re2O7 | RhO3 | RuO2 | Sb2O3 | Sb2O5 | Sc2O3 | Se | SeO2 | Sm2O3 | Ta2O5 | Tb2O3 | Tc2O7 | ThO2 | Tl2O | Tm2O3 | Trace | U3O8 | UO2 | WO3 | Y2O3 | Yb2O3

F (Fluorine)

Notes

Fluorine is used in super low melting frits. In combination with Li2O and small amounts of Bi2O3, boron frits containing fluorine can melt as low as 1100F (600C).

Generally, F is considered to exist in its elemental form in glasses and glazes. Its presence is time-dependent, it will volatilize as F2 gas if firing is extended. Fluorine is very reactive.
Materials like Cryolite and Fluorspar present complex challenges to model the chemistry of their firing.

F2 (or perhaps F) is often listed separately in analyses from manufacturers (not included in general LOI) because the hazardous nature of this gas (produced during firing).

A found recipe contains fluorine frit:

Is it a good idea to use that in a pottery studio?


Remove fluorine frit from a glaze

This picture has its own page with more detail, click here to see it.

It contains significant Frit P-25; it contains 1.8% fluorine! Are you really equipped to deal with fluorine gas in your studio? One answer is to substitute my own frits (which of course do not contain fluorine). I did the calculations in my account at insight-live.com (see the recipes side-by-side). In the formula, I substituted the F (fluorine) for a mix of CaO/MgO. In the recipe, I substituted Ferro Frit 3110 (it is also a high-sodium frit) for the P-25, then I juggled the rest of the recipe to match up the oxides. More Gerstley Borate supplies the lost B2O3, more ball clay supplies the lost Al2O3 and less silica is needed (because the ball clay brought along more). I ended up with a recipe that suspends better (more clay) and was able to eliminate the whiting. This recipe has a high thermal expansion, which means crazing. Would it not be easier to simply add a red stain to a clear glaze you already have that is working well on your clay bodies?

Links

Materials Fluorspar
Materials Sodium Fluosilicate
Materials Cryolite
URLs http://en.wikipedia.org/wiki/Fluorine
Fluorine at Wikipedia
Oxides Bi2O3 - Bismuth Oxide
Oxides Li2O - Lithium Oxide, Lithia

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy