Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Illmenite

Formula: FeTiO3

Ilmenite is a black colored heavy ore of iron and titanium. It is closely related to rutile. Material of up to 15% iron and other contaminants (and therefore 85% titanium) is called rutile whereas material of over 15% is called ilmenite (in reality ilmenite can contain up to 40% iron). Rutile is considered an impure form of titanium whereas ilmenite is considered as FeTiO3. Major other contaminants are magnesium and manganese.

Ilmenite occurs both an veins, disseminated deposits, or large masses. Thus according to the type of deposit the processed mineral will contain other things (i.e. apatite, syenite, diorite). It is mined in Quebec, Norway, New York state, Virginia, Africa and Australia.

It is now common for ilmenite operations to combine mine, mill, and smelter. The raw ore (often a "sand") is upgraded at the mill to produce a higher-grade ilmenite, near pure rutile (and often a zircon "concentrate"). There are two process to produce pure TiO2 from ilmenite (sulfate & chloride). Since the TiO2 industry is geared toward these requirements, ceramic users end up with the same grade.

Related Information

Links

URLs http://en.wikipedia.org/wiki/Ilmenite
Illmenite at Wikipedia
Materials Ilmenite
Minerals Hematite
The mineral form of iron(III) oxide. Used for the manufacture of steel but also available on finely

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy