Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Smectite

A highly plastic clay mineral related to montmorillonite (bentonite), more correctly, the name of the group on minerals that includes montmorillonite and other similar minerals. CAS# 1327-43-1 is magnesium aluminosilicate, a family of minerals. CAS# 12199-37-0 is smectite, a specific kind of magnesium aluminosilicate.

The following was obtained from Southern Clay Minerals:
Smectite is a platy clay mineral. Three properties make smectite unique:

Shape - Smectite is a very lamellar material. Individual platelets resemble a business card in terms of morphology.

Size - Naturally occurring smectite ranges in size from 0.25 microns up to 0.75 microns across its broadest dimension.

Charge - Smectite platelets have a negative ionic charge within the body of the platelet and a positive charge on the edge of the platelet.

Due to its particular combination of properties, smectite can provide a host of benefits in water-based coatings. Due to its ability to structure in aqueous media, it is a thickener in low to mid shear ranges. Oftentimes it can be used to reduce or replace (in combination with other thickeners) cellulosic thickeners. It also prevents settling and syneresis (phase separation). Smectite will act as a pigment spacer (U.S. Patent 5,700,319) to improve hiding in titanium dioxide pigmented systems. Smectite improves sag resistance while not affecting flow and levelling to the extent other mineral thickeners might. This is due to smectite's true thixotropy which affords a delay in the recovery of viscosity when shear is released as opposed to the pseudoplastic tendencies of other minerals which cause an immediate recovery of viscosity.

Related Information

Links

Materials 3B Clay
A fine-grained, tan burning, illitic stoneware with particulate and soluble salt impurities
Materials Veegum
A clay of incredibly small particle size. It has the highest plasticity of any known clay and acts as a suspending and gelling agent in slurries.
Materials Laponite RD
Glossary Porcelain
How do you make porcelain? There is a surprisingly simple logic to formulating them and to adjusting their working, drying, glazing and firing properties for different purposes.
Glossary Clay
What is clay? How is it different than dirt? For ceramics, the answer lies on the microscopic level with the particle shape, size and how the surfaces interact with water.
Minerals Hectorite
An uncommon fine-grained highly plastic clay mineral related to bentonite. Named after Hector, CA. F
Minerals Montmorillonite, Bentonite
A clay mineral of extremely small particle size and high plasticity. Raw bentonite is generally a pa
URLs http://www.minersoc.org/pages/gallery/claypix/smectite/YM01.html
One of many smectite micrographs at minersoc.org
URLs http://www.permont.com/
Southern Clay Products Smectite Minerals website
URLs http://en.wikipedia.org/wiki/Smectite
Smectite on WikiPedia
Typecodes Clay Minerals
The property of plasticity is evident in a wide array of materials of different mineralogy. In addition, many minerals are considered parent minerals to clays, they weather down to become these clays.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy