A clay mineral of extremely small particle size and high plasticity. Raw bentonite is generally a pale green, buff, cream, or grey material composed of the clay mineral montmorillonite. It is used to plasticize clay and porcelain bodies, often used in amounts of 1-5%.
Its origin can be traced to ancient volcanic eruptions where fine volcanic ash particles were carried by winds and deposited in discrete layers which altered over time from the glassy state to claystone. In North America, bentonites are mined in Montana, Wyoming, South Dakota and Saskatchewan and used in things like porcelain, toothpaste, tablets, cosmetics, oil drilling mud, oven cleaners, insecticides, putty, paint, ink, paper, polishes, cleansing agents, explosives, detergents, plastics and rubber.

This picture has its own page with more detail, click here to see it.
Notice the water just sits there in a little lake. It does not soak in because the bentonite gels in contact with the water and that gel acts as a non-permeable barrier. This water-barrier property of bentonite is a key to its use in many products. When ceramic bodies and glazes contain bentonite, they dry more slowly. In industrial settings, this can slow down production. But in studio settings, slower drying can enable more time to work with the material and more opportunities to intervene to make sure drying is happening evenly throughout.

This picture has its own page with more detail, click here to see it.
This disk has dried under heat (with the center part protected) for many hours. During that process it curled upward badly (flattening back out later). It is very reluctant to give up its water in the central protected section. Obviously it shrinks alot during drying and forms a network of cracks. When there are this many cracks it is difficult to characterize it, so a picture is best.

This picture has its own page with more detail, click here to see it.
Example of various materials mixed 75:25 with volclay 325 bentonite and fired to cone 9. Plasticities and drying shrinkages vary widely. Materials normally acting as fluxes (like dolomite, talc, calcium carbonate) are refractory here because they are fired in the absence of materials they react normally with.
| Materials |
Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying. |
| Materials |
Mineral Colloid BP
|
| Materials |
Gelwhite H
|
| Materials |
Bentone MA
|
| Materials |
Big Horn CE 200 Bentonite
|
| URLs |
http://www.sorptive.org/
Sorptive Mineral Institute for producers of absorbent clay mineral products |
| URLs |
http://www.handbookofmineralogy.org/pdfs/Montmorillonite.pdf
Montmorillonite mineralogy |
| URLs |
http://www.minersoc.org/pages/gallery/claypix/smectite/A-rose.html
Montmorillonite micrograph at minersoc.org |
| URLs |
http://en.wikipedia.org/wiki/Montmorillonite
Montmorillonite at Wikipedia |
| Minerals |
Smectite
A highly plastic clay mineral related to montmorillonite (bentonite), more correctly, the name of th |
| Minerals |
Hectorite
An uncommon fine-grained highly plastic clay mineral related to bentonite. Named after Hector, CA. F |
| Minerals |
Attapulgite, Palygorskite
Attapulgite is a magnesium aluminum silicate clay of very fine particle size. It is also known as Fu |
| Typecodes |
Clay Minerals
The property of plasticity is evident in a wide array of materials of different mineralogy. In addition, many minerals are considered parent minerals to clays, they weather down to become these clays. |
| Glossary |
Clay
What is clay? How is it different than dirt? For ceramics, the answer lies on the microscopic level with the particle shape, size and how the surfaces interact with water. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk