Allophane | Alunite | Amblygonite | Amorphous Silica | Anatase | Andalusite | Anorthite | Anorthosite | Aplite | Aragonite | Asbestos | Attapulgite, Palygorskite | Azurite | Baddeleyite | Ball Clay | Barytes, Barite | Bastnäsite | Bauxite | Berthierite | Beryl | Biotite | Boracite | Borate Minerals | Bornite | Brookite | Brucite | Calcite | Cassiterite | Celsian | Cerussite | Chalcedony | Chlorite | Chrysotile | Corundum | Dickite | Dolomite | Fayalite | Feldspar | Galena | Gibbsite | Granite | Gypsum | Hübnerite | Halloysite | Hectorite | Hematite | Hydroboracite | Illite | Illmenite | Iron Pyrite | K-Feldspar | Kaolinite | Kernite | Kyanite | Laterite | Lepidolite | Leucite | Limestone | Limonite | Magnesite | Magnetite | Malachite | Manganite | Mica | Microcline, Anorthoclase | Monazite | Montmorillonite, Bentonite | Mullite | Muscovite | Na-Feldspar | Nacrite | Nepheline | Nontronite | Oligoclase | Olivine | Organics | Pegmatite | Phlogopite Mica | Plagioclase | Potash Mica | Pyrophyllite | Quartz | Quartzite | Rutile | Sanidine | Saponite | Selenite | Sepiolite | Sericite | Serpentine | Shale | Sillimanite | Slate | Smectite | Soda Mica | Sodalite | Sphalerite | Steatite | Stibnite | Sylvite | Talc | Tremolite | Trona | Vanadinite | Willemite | Witherite | Zeolite

Steatite

Talc is also called steatite (it is a magnesium silicate hydrate). It is the main component of soapstone, it is the softest of all minerals (Mohs hardness of 1). Its silicate layers are weakly bound, this is the reason for the characteristic greasy or soapy feeling. It's color depends on the impurities (it can be colourless, white, grey, green, yellow or pink). It often it has a mother-of-pearl sheen.

Like dolomite and calcium carbonate, it has the curious property of being refractory when used pure but being a flux when combined with other materials.

Steatite is also a manufactured ceramic, a crystalline form of magnesium silicate (called synthetic steatite). It has relatively good strength and can service at temperatures up to 2,000°F (1180°C). It is much less expensive than sintered ceramics like alumina or zirconia. It's pressed density determines the porosity, compressive and flexural strength, conductivity and resistivity of the part being made.

Steatite is popular for making ceramic components where there is no need for tight dimensional tolerances, chemical purity or high mechanical stress - a common application is parts for electrical heaters.

Related Information


This picture has its own page with more detail, click here to see it.

Soapstone Steatite Carving


This picture has its own page with more detail, click here to see it.

Serpentine Soapstone

Links

URLs http://www.mondominerals.com/en/talc-production/mineralogy-geology/
Talc Mineralogy at Mondo Minerals
URLs http://www.associatedceramics.com/steatite.htm
Steatite properties page at Associated Ceramics
URLs http://en.wikipedia.org/wiki/Soapstone
Soapstone at Wikipedia
Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Glossary Refractory
In the ceramic industry, refractory materials are those that can withstand a high temperature without deforming or melting. Or can be sintered into super materials.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy