Alternate Names: Smithsonite, zinc spar
Formula: ZnCO3
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 64.91% | 1.00 | |
| CO2 | 35.09% | n/a | |
| Oxide Weight | 81.40 | ||
| Formula Weight | 125.40 | ||
| Materials |
Zinc Oxide
A pure source of ZnO for ceramic glazes, it is 100% pure with no LOI. |
| Hazards |
Zinc Compounds Toxicology
|
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| URLs |
http://en.wikipedia.org/wiki/Zinc_carbonate
Zinc carbonate at Wikipedia |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk