Volcanic Ash 2

Description: From Ron Roy's MDT

Oxide Analysis Formula Tolerance
CaO 5.08% 0.38
MgO 2.43% 0.26
K2O 1.38% 0.06
Na2O 4.33% 0.30
TiO2 0.59% 0.03
Al2O3 17.48% 0.73
SiO2 62.51% 4.42
Fe2O3 5.35% 0.14
MnO 0.07% -
LOI 0.77%n/a
Oxide Weight 421.61
Formula Weight 424.88

Related Information

Comparison of three volcanic ash chemistries


This picture has its own page with more detail, click here to see it.

Notice the amazing similarity between Mount St. Helen's and Mount Pinatubo ashes. And they are from opposite sides of the planet! Yet a common commercial material in North America, Navajo Pumice, is completely different.

Links

Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Materials Volcanic Ash
Powdered volcanic ash is used to make ceramic glazes, some varieties have a chemistry similar enough to glaze that high percentages can be employed.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy