Alternate Names: Vansil
Description: Calcium Metasilicate
Formula: CaSiO3
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 45.00% | 0.95 | |
| K2O | 0.10% | - | |
| MgO | 1.50% | 0.04 | |
| Na2O | 0.10% | - | |
| Al2O3 | 0.70% | 0.01 | |
| SiO2 | 50.00% | 0.99 | |
| Fe2O3 | 0.20% | - | |
| LOI | 1.60% | n/a | |
| Oxide Weight | 115.91 | ||
| Formula Weight | 117.79 | ||
This is the most common grade used in ceramic wall and floor tile, in glazes, and in frits for glazes and enamels. It also finds use in glaze and body stains, in bonds for vitrified grinding wheels, in electrical insulators, and as an auxiliary flux.
Different grades of the material vary in particle size (especially in the +325-200 range)
Density Mg/m3: 2.9
Weight (lbs/gal): 24.2
pH at 10% solids: 10-11
GE Brightness: 83
Hegman Fineness: 4
+325 mesh: 0.03%
W-10 has similar data except it is 19% +325 mesh (200 mesh grade). W-20 is 2.5% +325 mesh.
W-C-1 and DFSP are crushed.

This picture has its own page with more detail, click here to see it.
| Materials |
Wollastonite
|
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
| URLs |
http://www.vanderbiltminerals.com/product_categories/product_listing/category/paint-and-coatings-products-vansil-wollastonites
Vansil Wollastonite Data Sheet Links |
| URLs |
https://www.vanderbiltminerals.com/resources/Minerals_and_Chemical_for_Ceramics_and_Refractories_web.pdf
Vanderbilt Minerals for Ceramics Technical Sheet Includes Vansil, Pyrax, Peerless, Dixie, Veegum, Vanzan, Darvan. |