Unimin Potash Feldspar 300#

Oxide Analysis Formula Tolerance
CaO 0.05% 0.01
MgO 0.01% -
K2O 10.40% 0.66
Na2O 3.50% 0.34
TiO2 0.01% -
Al2O3 18.10% 1.06
SiO2 67.30% 6.67
Fe2O3 0.07% -
LOI 0.40%n/a
Oxide Weight 591.92
Formula Weight 594.30

Related Information

Links

Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.