Torrecid Frit MBK00007

Description: Zinc calcia magnesia titania low-alumina zero-boron frit

Oxide Analysis Formula Tolerance
ZnO 11.96% 0.29
MgO 4.03% 0.20
Al2O3 3.03% 0.06
Fe2O3 0.15% -
CaO 12.74% 0.45
SiO2 54.12% 1.78
Na2O 0.30% 0.01
TiO2 5.40% 0.13
K2O 2.68% 0.06
ZrO2 4.30% 0.07
SO4 1.29%n/a
Oxide Weight 194.57
Formula Weight 197.12

Notes

Matte, soft surface. High opacity. Affected by chemical attack.
Multicolor surface effects (likely due to high titanium content).

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy