1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

SG919 Laguna Cornwall Substitute

Oxide Analysis Formula Tolerance
SiO2 73.00% 9.26
Al2O3 16.00% 1.20
K2O 7.40% 0.60
Na2O 2.60% 0.32
CaO 0.60% 0.08
TiO2 0.20% 0.02
Oxide Weight 760.75
Formula Weight 760.75

Related Information

Links

Materials Cornwall Stone
URLs https://www.lagunaclay.com/_files/ugd/e5330f_7db9a3fbb7f34169a22ab4151512d40b.pdf
SG919 Cornwall Stone substitute from Laguna Clay
Article at their website comparing this with Cornwall stone and MFW30/G Spray Dried Flux.
URLs https://www.lagunaclay.com/_files/ugd/e5330f_deb4b5cce2c7486c98fcfc499603bd73.pdf
SG919 Cornwall Substitute SDS

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy