Alternate Names: Red Stone
Description: Plainsman Native Clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 0.32% | 0.02 | |
| CaO | 0.19% | 0.03 | |
| K2O | 2.57% | 0.21 | |
| MgO | 0.76% | 0.14 | |
| Na2O | 0.05% | 0.01 | |
| TiO2 | 0.65% | 0.06 | |
| Al2O3 | 13.54% | 1.00 | |
| P2O5 | 0.55% | 0.03 | |
| SiO2 | 72.26% | 9.06 | |
| Fe2O3 | 4.10% | 0.19 | |
| MnO | 0.01% | - | |
| LOI | 5.00% | n/a | |
| Oxide Weight | 715.66 | ||
| Formula Weight | 753.32 | ||
A natural high iron, mid-temperature stoneware clay of good plasticity. It is particulary well suited to oxidation bodies in the middle temperature ranges. It is very deep red at cone 7-8.
Fired Temperature, Cone 4 5 6 7 8 9
--------------------------------------
Fired Shrinkage: 3.1% 3.4% 3.7% 4.0% 4.2% 4.4%
Absorption: 6.4% 5.0% 4.0% 3.5% 3.0% 1.9%
Fired Strength:
(lbs/ square inch) 5100 5300 5600 5900 6400
Sieve Analysis Wet Washed
(Root of 2 series) +35 +48 +65 +100 +150# +200 +325
--------------------------------------------
0.0% 0.3% 2.4% 5.1% 7.6% 10.0% 22.2%
Texture: Sl. tooth
Plastic Index (1-10): 5
Green Strength (lbs/sqaure inch): 850
Dry shrinkage: 5.0
Dried density: 2.05
PCE: 15.5

This picture has its own page with more detail, click here to see it.
Plainsman Fire-Red (left) fired at cone 8,9,10,11 and 10R and Redstone (right) fired at cone 4,5,6,7,8.
| Materials |
M2 Red Stoneware
|
| Materials |
Fire-Red
|
| Materials |
Calvert Clay
|
| Typecodes |
Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically. |
| Pyrometric Cone Equivalent | 15 |
|---|