Pyrotrol 2004

Description: Andalusite/Pyrophyllite Ore

Oxide Analysis Formula Tolerance
K2O 0.20% 0.01
Na2O 0.20% 0.02
TiO2 0.40% 0.03
Al2O3 17.50% 1.00
SiO2 78.30% 7.59
Fe2O3 0.40% 0.01
LOI 2.80%n/a
Oxide Weight 565.37
Formula Weight 581.66

Notes

The Pyrotrol group of mineral products offers a controlled blend of milled Andalusite/Pyrophyllite ores designed to control strinkage in whiteware ceramic applications. Alumina contents are controlled to meet certain specifications. Pyrotrol produces an excellent kiln car wash and is an inexpensive coating material for facebrick production.

Related Information

Links

Materials Pyrotrol

Data

Bulk Density lbs/cu. ft. (Packed) 45
Pyrometric Cone Equivalent 26
Sieve Analysis Dry +200 mesh: 3.5%
Density (Specific Gravity) 2.80

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy