Precipitated Lime

Alternate Names: Precipitated Calcium Carbonate, PCC

Description: Synthetic calcium carbonate

Formula: CaCO3

Oxide Analysis Formula Tolerance
CaO 56.10% 1.00
CO2 43.90%n/a
Oxide Weight 56.10
Formula Weight 100.00

Notes

Made by heating calcium carbonate to remove the CO2 and make calcium hydroxide, adding water and purifying and then combining with the CO2 to precipitate the calcium carbonate back out leaving other impurities in the slurry. We are thus representing the chemistry as the theoretical pure CaCO3.

Ultrafine Nano PCC is also available (particles finer than 0.1 microns).

Related Information

Links

Minerals Limestone
Limestone forms by sedimentation, of coral and shells (biological limestone) or by the precipitation
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
URLs http://www.specialtyminerals.com/our-minerals/what-is-pcc/
PCC page at SpecialtyMinerals.com
Materials Quicklime
Materials Limestone

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy