Potassium Nitrate

Alternate Names: Niter, Saltpeter, KNO3

Formula: KNO3

Oxide Analysis Formula Tolerance
K2O 46.60% 1.00
LOI 53.40%n/a
Oxide Weight 94.20
Formula Weight 202.15

Notes

Prepared by the interaction of sodium nitrate and potassium chloride. It is used in glazes, glass and enamels for its oxidizing and fluxing properties.

Oxidation enamels usually contain 2-4% potassium or sodium nitrate to maintain oxidizing conditions during smelting to prevent reduction of compounds such as lead or antimony. Enamels with niter thus tend to froth during melting.

Related Information

Links

Materials Pearl Ash Calcined
Materials Pearl Ash
Materials Potasium Nitrate
Hazards Potassium Carbonate Toxicity
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
URLs http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc01/icsc0184.htm
Potassium Nitrate at ilo.org
URLs http://en.wikipedia.org/wiki/Potassium_nitrate
Potassium Nitrate at Wikipedia

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy