Pemco Frit Pb-742

Alternate Names: Frit Pb742

Description: Leaded zincless frit cone 08-1.

Oxide Analysis Formula Tolerance
CaO 4.50% 0.29
Na2O 3.60% 0.21
PbO 31.00% 0.50
ZrO2 1.00% 0.03
B2O3 13.00% 0.67
Al2O3 3.40% 0.12
SiO2 43.50% 2.61
Oxide Weight 360.79
Formula Weight 360.79

Notes

Blend with Pb-349 for intermediate temperatures. Pb-63 has slightly more zirconia.

Similar to alternatives but has small amount of ZrO2 smelted in.

Related Information

Links

Materials General Frit GF-27
Materials Ferro Frit 3576
Materials Ferro Frit 3493
Materials Ferro Frit 3485
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit Pb-63
Materials Fusion Frit FL-28
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.5 x 10-6 (40-450C)
Frit Melting Range (C) 1350-1450F
I.F.P. (celsius) 585C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy