General Frit GF-27

Alternate Names: Frit 27, Frit GF27

Description: Medium lead frit cone 06-04 all-fritted hobby/artware glazes

Oxide Analysis Formula Tolerance
CaO 4.40% 0.28
Na2O 3.60% 0.21
PbO 31.50% 0.51
ZrO2 1.00% 0.03
B2O3 13.00% 0.67
Al2O3 3.40% 0.12
SiO2 43.50% 2.61
Oxide Weight 361.64
Formula Weight 361.64

Related Information

Links

Materials Pemco Frit Pb-742
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3576
Materials Fusion Frit FL-28
Materials Hommel Frit 373
Materials Ferro Frit 3493
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.90
Frit Softening Point 1400F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy