Description: Medium lead sodium borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 6.10% | 0.33 | |
| PbO | 44.50% | 0.67 | |
| B2O3 | 13.80% | 0.67 | |
| SiO2 | 35.60% | 1.99 | |
| Oxide Weight | 335.84 | ||
| Formula Weight | 335.84 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Hommel Frit 520
|
| Materials |
General Frit 400F
|
| Materials |
Douteux Frit LB75
|
| Materials |
Hommel Frit 373
|
| Materials |
Pemco Frit Pb-742
|
| Materials |
Stain 6373
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.70 |
|---|---|
| Frit Melting Range (C) | 1300F |