Pemco Frit P-688

Alternate Names: Frit 688, Frit P688

Description: LEADLESS FRIT

Oxide Analysis Formula Tolerance
BaO 10.60% 0.11
CaO 15.80% 0.45
K2O 3.00% 0.05
MgO 4.30% 0.17
Na2O 1.60% 0.04
ZnO 8.70% 0.17
Al2O3 7.00% 0.11
SiO2 49.00% 1.31
Oxide Weight 160.77
Formula Weight 160.77

Notes

Used for partially-fritted, cone 9-12 opaque sanitaryware glazes.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-108
Materials Hommel Frit 28F198
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.0 x 10-6 (50-450C)
Frit Melting Range (C) 1550-2100F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy