Pemco Frit P-3E12

Alternate Names: Frit 3E12, Frit P3E12

Description: Semi-opaque all-fritted glaze for cone 02-4

Oxide Analysis Formula Tolerance
CaO 6.20% 0.28
K2O 6.70% 0.18
MgO 1.40% 0.09
Na2O 3.00% 0.12
ZnO 10.10% 0.32
ZrO2 3.10% 0.06
B2O3 4.90% 0.18
Al2O3 13.20% 0.33
SiO2 51.40% 2.20
Oxide Weight 257.17
Formula Weight 257.17

Notes

A lower-expansion version of P-1J81

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-1J81
Materials Fusion Frit FZ-164
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.80
Co-efficient of Linear Expansion 7.8 x 10-6 (50-450C)
Frit Softening Point 1650F
Frit Melting Range (C) 1620-1720F
I.F.P. (celsius) 658C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy