Pemco Frit P-1836

Alternate Names: Frit 1836, Frit P1836

Description: Leadless, high zinc, all-fritted glaze

Oxide Analysis Formula Tolerance
BaO 6.70% 0.11
CaO 7.10% 0.32
K2O 1.10% 0.03
Na2O 3.80% 0.16
ZnO 12.30% 0.38
B2O3 3.10% 0.11
Al2O3 7.10% 0.18
SiO2 58.80% 2.48
Oxide Weight 253.59
Formula Weight 253.59

Notes

Used on regular and fast-fire wollastonite and talc bodies.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.1 x 10-6 (50-450C)
Frit Melting Range (C) 1500-1700F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy