1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Opeal OP-3 Ball Clay

Description: Super-white ball clay

Oxide Analysis Formula Tolerance
SiO2 50.60% 2.51
Al2O3 34.20% 1.00
Fe2O3 0.72% 0.01
TiO2 0.43% 0.02
CaO 0.06% -
MgO 0.08% 0.01
K2O 1.26% 0.04
Na2O 0.11% 0.01
LOI 12.54%n/a
Oxide Weight 260.85
Formula Weight 298.25

Notes

Excellent plasticity and reasonable particle distribution and it can improve the speed and quality when making semi-finished ceramic products. Application in high-grade polished tiles, porcelain tiles, sanitary ware,etc .

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.
URLs http://www.opeal.com.cn/english/products_op03.htm
OP-3 Ball Clay information

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy