1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Noor Hematite

Alternate Names: Egyptian Hematite

Oxide Analysis Formula Tolerance
SiO2 11.50% 2.65
TiO2 0.30% 0.05
Al2O3 3.10% 0.42
Fe2O3 76.80% 6.65
MnO 0.30% 0.06
MgO 0.70% 0.24
CaO 2.30% 0.57
Na2O 0.10% 0.02
K2O 0.15% 0.02
P2O5 1.50% 0.15
LOI 0.10%n/a
Oxide Weight 1,341.07
Formula Weight 1,378.28

Notes

The analysis shown in an average of 6 samples tested in 2002.
This iron can be as high as 88% and as low as 61%.

Related Information

Links

Materials Hematite
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy