Muscovite Mica

Formula: KAl2(Si3Al)O10(OH,F)2

Oxide Analysis Formula Tolerance
K2O 11.80% 1.00
Al2O3 38.36% 3.00
SiO2 45.21% 6.01
F 0.95% 0.40
LOI 4.07%n/a
Oxide Weight 768.93
Formula Weight 801.55

Related Information


This picture has its own page with more detail, click here to see it.

Aquamarine Muscovite Albite


This picture has its own page with more detail, click here to see it.

Almand Cleveland Muscov-ite


This picture has its own page with more detail, click here to see it.

Muscovite Stone2


This picture has its own page with more detail, click here to see it.

Muscovite Mica

Links

URLs http://www.webmineral.com/data/Muscovite.shtml
Muscovite at webmineral.com
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy