Description: High boron zero silicate refractory calcia alumina frit

Oxide Analysis Formula Tolerance
B2O3 40.00% 1.34
Al2O3 33.00% 0.76
CaO 24.00% 1.00
Oxide Weight 226.74
Formula Weight 226.74

Notes

Although this frit is very high in boron, it is a refractory (this might be a surprise to ceramic technicians who are accustomed to the use of boron as a powerful flux). Frits of this type have been in use to stop the penetration of aluminum in refractories since 1958 (by Carborundum Co., Metaullics Inc., Ceradyne, H-W Refractories (now ANH), and AP Green, and others). The original patent holder for these frits was Kaiser Aluminum Corp.

They are about ~1% soluble after 90 min in ~25 C water. In this way they can be used in castable cements where any appreciable amount of soluble boric oxide would retard Calcium Aluminate cement almost indefinitely.

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Materials Matrix Frit B70-A
Materials Calcium Aluminate Cement
Oxides B2O3 - Boric Oxide

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy