1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Matrix Frit B70-A

Description: High boron zero silicate calcia alumina frit

Oxide Analysis Formula Tolerance
B2O3 70.00% 4.27
Al2O3 24.00% 1.00
CaO 4.00% 0.30
Oxide Weight 416.50
Formula Weight 416.50

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.