Kuncice Dolomite

Description: Unknown

Oxide Analysis Formula Tolerance
SiO2 1.30% 0.02
Al2O3 0.30% -
K2O 0.40% -
MgO 19.90% 0.46
CaO 32.00% 0.53
LOI 46.00%n/a
Oxide Weight 50.45
Formula Weight 93.42

Related Information

Links

Materials Dolomite
An inexpensive source of MgO and CaO for ceramic glazes, also a highly refractory material when fired in the absence of reactant fluxes.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy