KaoPearl CNL30 Kaolin

Alternate Names: KaoPearl, CNL30

Oxide Analysis Formula Tolerance
Fe2O3 0.60% 0.01
K2O 1.30% 0.04 +/- 0.25
SiO2 47.50% 2.18
Al2O3 37.00% 1.00
TiO2 0.05% -
Na2O 0.15% 0.01
CaO 0.05% -
MgO 0.30% 0.02
Oxide Weight 239.70
Formula Weight 239.70

Notes

An Imerys product, apparently a possible replacement for Super Standard Porcelain. Available in North America. The data sheet indicates a production site in Cornwall, UK. Their first data sheet was released in March 2021.

The K2O varies somewhat.

Related Information

Links

Materials Super Standard Porcelain
Materials Grolleg Kaolin
A white burning kaolin from the UK, commonly used in porcelain bodies and as a glaze suspender. Sticky when wet, low plasticity.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
URLs https://digitalfire.com/4sight/datasheets/KaoPearlCNL30.pdf
KaoPearl CNL30 Data Sheet
Release date: March 2021

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy