Alternate Names: Kaolen 171
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.26% | 0.01 | |
| MgO | 0.62% | 0.04 | |
| K2O | 0.12% | - | |
| Na2O | 0.20% | 0.01 | |
| TiO2 | 0.28% | 0.01 | |
| Al2O3 | 35.55% | 1.00 | |
| SiO2 | 46.87% | 2.24 | |
| Fe2O3 | 1.90% | 0.03 | |
| LOI | 14.20% | n/a | |
| SO4 | 0.38% | n/a | |
| Oxide Weight | 246.18 | ||
| Formula Weight | 288.20 | ||
Available in minus 20cm, -100 microns, -75 microns.
| Materials |
Kaolin 115
|
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Materials |
Kaolin 143
|
| Materials |
Kaolin 114
|
| Materials |
Kaolin 113
|
| Materials |
Kaolin 111
|
| Materials |
Kaolin 151
|
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk