1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

IXL 45R

Description: Low temperature red earthware, terra cotta

Oxide Analysis Formula Tolerance
CaO 0.81% 0.12
K2O 3.60% 0.31
MgO 1.88% 0.38
Na2O 1.40% 0.18
TiO2 0.59% 0.06
Al2O3 14.50% 1.16
P2O5 0.15% 0.01
SiO2 64.40% 8.72
Fe2O3 5.18% 0.26
MnO 0.07% 0.01
LOI 6.50%n/a
Oxide Weight 753.01
Formula Weight 805.36

Notes

A very plastic low temperature red burning terra cotta clay that was mined, by I-XL Industries, near Elkwater, Alberta, Canada. It was originally described as a clay "consisting largely of illite and free silica with a bit of free siderite as small concretions or crystals between the grains". That being said, in physical terms it was a low-temperature terra cotta clay, vitrifying by cone 1 because of the presence of significant feldspar. It was fairly high in soluble salts and required barium carbonate to precipitate these in production bodies. Hundreds of thousands of tons were used to make brick and vitrified pipe. Plainsman Clays also used this for many years to make terra cotta clay bodies and as a source of feldspar in middle-temperature red and brown stonewares. No longer available.

In later years BGP and 98 Mix were used for similar purposes.

Related Information

IXL 45R fired bars


This picture has its own page with more detail, click here to see it.

Fired from cone 5 (top) down to cone 1 (bottom).

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Materials IXL 45D
Materials IXL 45F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy