Hommel Frit 498

Oxide Analysis Formula Tolerance
K2O 3.23% 0.06
Na2O 1.70% 0.05
CaO 16.91% 0.52
MgO 5.25% 0.22
BaO 11.56% 0.13
ZnO 0.95% 0.02
Al2O3 7.68% 0.13
SiO2 52.72% 1.51
Oxide Weight 172.27
Formula Weight 172.27

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.1 x 10-6
Frit Melting Range (C) 1820F