G200 Old Blend Feldspar

Alternate Names: MFEL S3470 Blend

Oxide Analysis Formula Tolerance
Al2O3 18.20% 1.00
CaO 1.00% 0.10
Fe2O3 0.08% -
K2O 10.50% 0.63
Na2O 3.00% 0.27
SiO2 66.80% 6.26
LOI 0.20%n/a
Oxide Weight 560.45
Formula Weight 561.58

Notes

To be as similar as possible to the old G-200 feldspar, Laguna Clays blended 3 parts Minspar and 7 parts G-200 HP to produce this material.
However G-200HP was then discontinued so Laguna Clays began importing Mahavir Feldspar from India.

Related Information

Old Blend Feldspar. What is that?


This picture has its own page with more detail, click here to see it.

Laguna Clay sells a substitute for the no-longer-available G200 feldspar. G200 HP is higher in K2O and lower in CaO than G200, Minspar is an ideal addition since it's K2O is much lower and CaO much higher. A 7:3 G200HP:Minspar mix produces a chemistry that is remarkably close (on paper) to G200. They label this blend "Old Blend". They also list a product called "New Potash" in their pricelist, that is G200 HP.

Links

Materials G-200 Feldspar
Materials G200 HP Feldspar
Materials Mahavir Potash Feldspar
Materials G-200 EU Feldspar
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy