Fusion Frit FZ-915

Description: Bismuth frit

Oxide Analysis Formula Tolerance
SiO2 22.00% 2.86
B2O3 15.50% 1.74
Na2O 4.00% 0.50
K2O 2.50% 0.21
ZnO 3.00% 0.29
Bi2O3 53.00% 0.89
Oxide Weight 781.80
Formula Weight 781.80

Notes

This is the only bismuth frit that we know of that is available to potters in North America. Their data sheet gives an approximate analysis of 2-6% K2O, 1-4% Na2O, 2-4% ZnO, 15-20% B2O3, 17-22% SiO2, 50-60% Bi2O3. This was not reconcilable with a data sheet that we had, so numbers from that sheet have been pulled just inside their published boundaries. It is not completely clear whether the chemistry is variable because of production issues or the numbers are getting muddled in trade secret initiatives.

This frit is practical only for very specialized uses. The reason is this costs $30/lb (in 2020). That is $1500 per 50/lb bag and $60,000 for the minimum order of 2000 lbs.

Related Information

Fusion Bismuth Frit FZ -915 fired to cone 6


This picture has its own page with more detail, click here to see it.

The pure frit powder was simply melted in this tile.

Links

URLs https://johnbrittpottery.com/shop/experiments-in-manganese-gold-and-iridescent-glazes-in-electric-oxidation-cones-6-12/
John Britt's work with a bismuth frit
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Oxides Bi2O3 - Bismuth Oxide
Materials Bismuth Subnitrate
Materials Bismuth Oxide
Bismuth is a very strong flux that enables glass melts lower than any other, even lead. However its price limits its utility to highly specialized products.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy