Fusion Frit F-5

Alternate Names: Fusion Frit F5

Description: Strontium Barium flux

Oxide Analysis Formula Tolerance
CaO 10.22% 0.49
BaO 11.73% 0.21
Na2O 1.72% 0.07
K2O 2.42% 0.07
SrO 6.04% 0.16
Al2O3 5.14% 0.14
B2O3 6.12% 0.24
SiO2 56.62% 2.54
Oxide Weight 269.99
Formula Weight 269.99

Related Information

Links

URLs http://www.fusionceramics.com/
Fusion Ceramics Frit Website
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.13 x 10-6
Frit Softening Point 1800F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy