Fusion Frit F-380

Alternate Names: Frit F380

Description: Barium leadless frit

Oxide Analysis Formula Tolerance
BaO 18.50% 0.40
CaO 6.60% 0.39
Na2O 3.80% 0.20
B2O3 8.50% 0.41
Al2O3 6.00% 0.20
SiO2 56.00% 3.11
Oxide Weight 331.76
Formula Weight 331.76

Related Information

Frit melt fluidity comparison - 1300F


This picture has its own page with more detail, click here to see it.

Fired at 350F/hr to 1300F and held for 15 minutes. Some are still burning off carbon (which seems strange). There are two early leaders: Ferro frit 3110 and Fusion frit F75 are starting to deform (they have almost the same chemistry). Amazingly, these two frits have low boron, they rely on high soda as the flux.

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy