Description: Strontium frit base for cone 5-6 glazes

Oxide Analysis Formula Tolerance
CaO 11.00% 0.57
K2O 1.20% 0.04
Li2O 0.40% 0.04
Na2O 4.90% 0.23
SrO 4.50% 0.13
B2O3 6.00% 0.25
Al2O3 11.50% 0.33
SiO2 60.50% 2.92
Oxide Weight 290.10
Formula Weight 290.10

Related Information

Links

Materials Ferro Frit 3292
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 389
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.07 x 10-6
Frit Softening Point 1800F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy