Description: Low melting high expansion sodium borosilicate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 2.44% | 0.14 | |
| K2O | 5.86% | 0.20 | |
| Na2O | 12.72% | 0.66 | |
| B2O3 | 14.50% | 0.67 | |
| Al2O3 | 9.19% | 0.29 | |
| SiO2 | 55.30% | 2.96 | |
| Oxide Weight | 321.73 | ||
| Formula Weight | 321.73 | ||
Useful for raku glazes
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 4125
|
| Materials |
MOK 3 Borax frit
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |