Ferro Frit 4125

Alternate Names: Ferro Frit 5325

Description: Low melting high expansion sodium borosilicate fluorine frit

Oxide Analysis Formula Tolerance
CaO 2.36% 0.14
K2O 2.59% 0.09
Na2O 14.77% 0.77
F 2.72% 0.47
Al2O3 7.97% 0.25
B2O3 13.81% 0.64
SiO2 55.77% 3.01
Oxide Weight 324.87
Formula Weight 324.87

Notes

Was known as Ferro Frit 5325

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit 5325
Materials Ferro Frit 5325P
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy