Frit VO 6270

Description: Reimbold & Strick stoneware tableware frit < 1050C

Oxide Analysis Formula Tolerance
Na2O 3.00% 0.14
SiO2 43.00% 2.08
SrO 13.00% 0.36
K2O 2.00% 0.06
BaO 4.00% 0.08
B2O3 25.00% 1.04
ZnO 10.00% 0.36
Oxide Weight 290.66
Formula Weight 290.66

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 54 x 10-7 (20-400C)
Frit Softening Point 660C
Glass Transition Temperature 600C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy