Ferro Frit 4193

Description: Transparent hard barium zinc borosilicate leadless frit

Oxide Analysis Formula Tolerance
BaO 2.04% 0.04
CaO 9.42% 0.54
Na2O 3.97% 0.21
ZnO 2.78% 0.11
B2O3 14.25% 0.66
SiO2 57.73% 3.09
K2O 2.94% 0.10
Al2O3 6.87% 0.22
Oxide Weight 321.94
Formula Weight 321.94

Notes

Supposedly this used to be Frit 938 however, while very similar this only has half the amount of BaO.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 938
Materials Ferro Frit DA4193
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 1040-1100C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy