Ferro Frit 4049

Description: High boron low lead frit

Oxide Analysis Formula Tolerance
BaO 0.03% -
CaO 6.70% 0.40
MgO 0.23% 0.02
Na2O 4.03% 0.22
ZnO 0.20% 0.01
SrO 0.07% -
PbO 6.17% 0.09
B2O3 24.07% 1.15
SiO2 50.80% 2.82
K2O 7.40% 0.26
Oxide Weight 332.71
Formula Weight 332.71

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.