| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 0.03% | - | |
| CaO | 0.42% | 0.01 | |
| K2O | 0.05% | - | |
| Na2O | 0.14% | - | |
| PbO | 0.26% | - | |
| ZnO | 96.00% | 0.99 | |
| B2O3 | 0.27% | - | |
| Al2O3 | 0.29% | - | |
| SiO2 | 2.89% | 0.04 | |
| Oxide Weight | 84.25 | ||
| Formula Weight | 84.25 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |