Ferro Frit 3185

Alternate Names: F3185

Description: Low melting alkali borate bonding frit for abrasives

Oxide Analysis Formula Tolerance
Na2O 7.70% 1.00
B2O3 38.20% 4.42
SiO2 54.10% 7.25
Oxide Weight 805.19
Formula Weight 805.19

Related Information

At 1700F the fast fire frits show an important difference


12 frits melting at 1700F

This picture has its own page with more detail, click here to see it.

These were 10g balls melted using our GBMF test, the tile they are being fired on is a grogged stoneware clay. A few of the more interesting ones here are frit 3470 lead zinc, 3185 super high boron, CC257 high barium, FR003 high alkali and F49 and FR001 opacifieds. Notice how early and vigorously some are melting. But notice 557 and 556, they aren’t doing anything - that is not by accident. These are fast-fire frits, they are designed to melt later and more quickly. This is only 1700F, since no one fires this low it makes sense that if a glaze has not started melting it will be able to pass escaping gases of decomposition. This avoids the bubbles and surface defects these cause, as 3185, CC257 and 3470 are already demonstrating. What about FR002, FR002 and 3565, they are melting and look fine? They have higher surface tension and much less contact with the body generating the gases.

Links

Materials Fusion Frit F-245
Materials Fusion Frit F-367
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3226
Materials General Frit GF-143
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Bonding Frits
Also called glass frits, these melt at very low temperatures (e.g. 500C). They are used to bond together materials that can withstand some heat (e.g. abrasives, ceramics, non-oxide ceramics, metals). And as a surface-smoothing agent. The main product properties are melting temperature and thermal expansion. The powders are mixed with binders, applied and then heated up and down to create the bond.

Data

Co-efficient of Linear Expansion 6.10
Frit Melting Range (C) 1350F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy