Fusion Frit F-367

Alternate Names: Fusion Frit F367

Description: Bond Frit

Oxide Analysis Formula Tolerance
Na2O 7.80% 1.00
B2O3 38.40% 4.39
SiO2 53.80% 7.12
Oxide Weight 794.87
Formula Weight 794.87

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3185
Materials General Frit GF-143
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 4.18 x 10-6
Frit Softening Point 1475F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy