Esmalglass Frit FT 8547

Alternate Names: Esmalglass Frit 8547

Oxide Analysis Formula Tolerance
P2O5 0.10% -
K2O 5.40% 0.12
Fe2O3 0.10% -
Na2O 0.90% 0.03
Al2O3 7.50% 0.16
SiO2 60.50% 2.16
MgO 1.20% 0.06
CaO 14.90% 0.57
ZnO 7.90% 0.21
BaO 0.10% -
LOI 0.60%n/a
Oxide Weight 211.76
Formula Weight 213.04

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 1090C
Frit Melting Range (C) 1170C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy