1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Esmalglass Frit FM 86

Oxide Analysis Formula Tolerance
MgO 0.50% 0.03
Fe2O3 0.10% -
K2O 4.00% 0.09
ZrO2 0.60% 0.01
SiO2 45.90% 1.64
ZnO 11.90% 0.31
Al2O3 19.60% 0.41
P2O5 0.10% -
Na2O 1.50% 0.05
PbO 0.70% 0.01
CaO 12.80% 0.49
SrO 0.30% 0.01
BaO 0.80% 0.01
LOI 0.50%n/a
Oxide Weight 212.30
Formula Weight 213.37

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Softening Point 855C
Frit Melting Range (C) 1180C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy